Process Mineralogy of the Tailings from Llallagua: Towards a Sustainable Activity
Ver/ Abrir
Registro completo
Mostrar el registro completo DCAutoría
Alfonso, Pura; Ruiz, Miguel; Zambrana, Rubén Néstor; Sendrós, Miquel; García Valles, Maite; Anticoi Sudzuki, Hernán Francisco; Sidki Rius, Nor; Salas, AntonioFecha
2022-02-07Derechos
© 2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.
Publicado en
Minerals 2022, 12(2), 214
Editorial
MDPI
Palabras clave
Process mineralogy
Tailings
Cassiterite
REE
Mineral liberation
Quantitative mineralogy
Resumen/Abstract
There are significant tin reserves in the dumps and tailings from Llallagua. Currently, this waste is being processed using gravity concentration or a combination of gravity concentration with a final stage of froth flotation. A process mineralogy study of the tailings and their products after processing in Llallagua was carried out to determine the failings of the processing system in order to contribute to designing an improved new processing scheme. The mineralogy of the feed tailings, concentrate, and final tailings was determined by X-ray diffraction, scanning electron microscopy, and mineral liberation analysis. The tailings were composed of quartz, tourmaline, illite, K-feldspar, plagioclase, cassiterite, rutile, zircon, and monazite. The concentrate essentially contains cassiterite (57.4 wt.%), tourmaline, quartz, hematite, rutile and rare earth minerals, mainly monazite and minor amounts of xenotime and florencite. The concentrate contained 52?60 wt.% of SnO2 and 0.9?1.3 wt.% REE. The final tailings contained 0.23?0.37 wt.% SnO2 and 0.02 wt.% of Rare Earth Elements (REE). Only 57.6 wt.% of cassiterite from the concentrate was liberated. The non-liberated cassiterite was mainly associated with quartz, tourmaline, and rutile. The average grain size of monazite was 45 µm and 57.5 wt.% of this was liberated. In other cases, it occurs in mixed particles associated with tourmaline, quartz, cassiterite, and muscovite. To improve the sustainability of this mining activity, the concentrate grade and the metal recovery must be improved. Reducing the particle size reduction of the processed tailings would increase the beneficiation process rates. In addition, the recovery of the REE present in the concentrate as a by-product should be investigated